李淑欣,女,畢業於蘭州理工大學,從事腐蝕疲勞研究工作。

基本信息

個人簡介

李淑欣 蘭州理工大學副教授(Associate Professor li Shuxin),碩士生導師,1975年11月生。2003年於蘭州理工大學化工機械專業獲碩士學位,2007年3月於華東理工大學化工過程機械專業獲博士學位。2010年2月至2011年8月作為高級研究員在英國Sheffield Hallam University 從事腐蝕疲勞研究工作。

李淑欣教授李淑欣教授

研究方向
1)奧氏體不鏽鋼疲勞性能
2)結構強度和可靠性
3)擴散連線技術
4)壓力管道安全評定和風險分析

代表性論文

1. Li S X, Li L, Yu S R, Akid R, Xia H B. Investigation of intergranular corrosion of 316L stainless steel diffusion bonded joint by electrochemical potentiokinetic reactivation. Corrosion Science. 2011, 53: 99-104.(SCI/EI)
2. LI Y J, Xuan F Z, Li S X, Tu S T. Quality Evaluation ofDiffusion Bonded Joints by Electrical Resistance Measuring and Microscopic Fatigue Testing. Chinese Journal of Mechanical Engineering, 2011,24, 187-194. (EI)
3. Li S X, Zeng H L, Yu S R. A method of probabilistic analysis for steel pipeline with correlated corrosion defects. Corrosion science, 2009, 51: 3050-3056. (SCI/EI)
4. Li S X, Yu S R. Predicting corrosion remaining life of underground pipelines with a mechanically-based probabilistic model. J.Petroleum Sci.& Eng. 2009, 65: 162-166. (SCI/EI)
5. Li S X, Xuan F Z, Tu S T. Microstructural evolution and interfacial failure mechanism in 316LSS diffusion bonded joints. Mater. Sci. Eng. A, 2008, 491: 488-491. (SCI/EI)
6. Li S X, Xuan F Z, Tu S T. Fatigue damage of stainless steel diffusion-bonded joints Mater. Sci. Eng. A, 2008, 480: 125-129. (SCI/EI)
7. Li S X, Xuan F Z, Tu S T. In Situ observation of interfacial fatigue crack growth in diffusion bonded joints of austenitic stainless steel. J. Nucl. Mater. 2007, 366:1-7. (SCI/EI)
8. Li S X, Tu S T, Xuan F Z. A probabilistic model for prediction of bonding time in diffusion bonding. Mater. Sci. Eng. A, 2005, 407(1-2), 250-255. (SCI/EI)
9. Li S X, Tu S T, Zheng D W. Monte-Carlo Techniques in Modern Mechanics, Proceeding of Traditional Mathematics and Mechanics, May 22-28, 2004,Messini, Greece. (ISTP)
10. Li L, Li S X, Yu S R. Microstructure and intergranular corrosion of 316L stainless steel diffusion
bonded joint. Page 1-7. Proceeding of 2011 international symptom on structural integrity. October 21-24, 2010, Shanghai, China.
11. 李淑欣, 軒福貞塗善東俞樹榮. 316LSS擴散連線接頭界面疲勞裂紋擴展行為. 材料科學與工藝,2010,18(1): 141-144. (EI)
12. 李淑欣, 塗善東, 軒福貞. 奧氏體不鏽鋼擴散連線界面疲勞斷裂的微觀機理. 材料研究學報,2007, 21:152-155. (EI)
13. 軒福貞,張波,李淑欣. 電阻法用於擴散焊接頭微孔缺陷評價的數值模擬. 焊接學報,2007, 28(4): 9-12 (EI).
14. 李淑欣,塗善東,軒福貞. 表面粗糙度對擴散連線孔隙閉合時間的影響. 中國機械工程, 2006, 17(14): 1512-1515. (EI)
15. 孫寶財,李淑欣,曾海龍,俞樹榮. 基於改進BP算法的腐蝕管道剩餘強度評價. 腐蝕學報(2011,已接受).